daveycrockett

Ordered some of these today. What are you that use these using to glue the inserts in with?

southpawshooter

JB weld or Gorilla flexible super glue
Scott F >>--->   @

"if the wood don't fly the bunny don't die" - Stone Knife, JLMBH 2008

Proud member of Team Pink

daveycrockett

QuoteOriginally posted by southpawshooter:
JB weld or Gorilla flexible super glue
Thanks

JRY309

I just used some AAE 24 hr. epoxy,same as I use on my inserts for carbons.

daveycrockett

Anybody try the blue low heat hot melt?   :campfire:

RLA

(Anybody try the blue low heat hot melt?    :campfire: )  

Yes, that's what I've been using with good results.

TOEJAMMER

Always use the low heat hot melt and have never had an insert pull out.

daveycrockett


JamesKerr

I use Easton's hot melt glue. It holds much better for me than Bohning's hot melt and it melts at a lower temperature.
James Kerr

threeunder

Hot melt for me.  Never slipped an insert.
Ken Adkins

Never question a man's choice in bows or the quality of an animal he kills.  He is the only one who has to be satisfied with either of those choices.