Hello guys i need help .I buy this epoxy .
Two ways, the first is the ratio of 1:1 the other is 2:1.
At the instruction manual explains that when we use the 2:1 ratio improves the temperature resistance and improves physical properties. All this I ask because I bonding process performed at room temperature 24-48 hours . Basically this is a question for all bowyers who use this epoxy resin
When I do glue up's I always use the 1:1 ratio and have no problems so far... My 2 cents
I suggest posting this on the bowyers forum, alot of info there.
The glue should be cured by now.